C276 Nickel Technical Data
| Nickel |
Balance |
| Cobalt |
2.5 Max |
| Chromium |
15.5 |
| Molybdenum |
16.0 |
| Tungsten |
3.75 |
| Iron |
5.5 |
| Silicon |
0.08 Max |
| Manganese |
1.0 Max |
| Carbon |
0.01 Max |
| Density |
0.321 lb/in3 |
| Tensile
Strength |
115500 psi |
| Tensile
Strength, Yield |
54600 psi |
| Elongation
at Break |
60 % |
| Modulus
of Elasticity |
29700 ksi |
| Poisson's
Ratio |
0.307 |
| Shear
Modulus |
11500 ksi |
| Magnetic
Permeability |
1.0002 |
| Specific
Heat Capacity |
0.102 BTU/lb-°F |
| Thermal
Conductivity |
68 BTU-in/hr-ft2-°F |
| Melting
Point |
2420
- 2500 °F |
<<