| Density |
0.305 lb/in3 |
| Tensile
Strength, |
131000 psi |
| Tensile
Strength, Yield |
71100 psi |
| Elongation
at Break |
48.5 % |
| Modulus
of Elasticity |
30200 ksi |
| Modulus
of Elasticity at Elevated Temperature |
18300 ksi |
| Electrical
Resistivity |
0.000129 ohm-cm |
| Electrical
Resistivity 100°C (212°F) |
0.000132 ohm-cm |
| CTE,
linear 20°C |
7.11 μin/in-°F |
| CTE,
linear 1000°C |
9.67 μin/in-°F |
| Specific
Heat Capacity |
0.098 BTU/lb-°F |
| Specific
Heat Capacity 100°C (212°F) |
0.102 BTU/lb-°F |
| Thermal
Conductivity |
68 BTU-in/hr-ft2-°F |
| Thermal
Conductivity 100°C (212°F) |
75.6 BTU-in/hr-ft2-°F |
| Melting
Point |
2350-2460 °F |