5086-H32 Aluminum Data

 

 

Aluminum Balance
Chromium 0.05 - 0.25
Copper 0.1 max
Iron 0.5 max
Magnesium 3.5 - 4.5
Manganese 0.2 - 0.7
Remainder Each 0.05 max
Remainder Total 0.15 max
Silicon 0.4 max
Titanium 0.15 max
Zinc 0.25 max

 

 

Density 0.0961 lb/in3
Hardness, Brinell 87
Tensile Strength 47000 psi
Tensile Yield Strength 37000 psi
Elongation at Break 10 %
Modulus of Elasticity 10300 ksi
Compressive Strength 47100 psi
Compressive Modulus 10500 ksi
Poisson's Ratio 0.33
Shear Modulus 3830 ksi
Shear Strength 27000 psi
Electrical Resistivity 5.49e-006 ohm-cm
CTE, linear 68°F 13.2 μin/in-°F
CTE, linear 250°C 14.3 μin/in-°F
Specific Heat Capacity 0.215 BTU/lb-°F
Thermal Conductivity 870 BTU-in/hr-ft2-°F
Melting Point 1085 - 1185 °F
<<