5052-H32 Aluminum Data
| Aluminum |
Balance |
| Chromium |
0.15
- 0.35 |
| Copper |
0.1
max |
| Magnesium |
2.2
- 2.8 |
| Manganese |
0.1
max |
| Remainder
Each |
0.05
max |
| Remainder
Total |
0.15
max |
| Silicon
+ Iron |
0.45
max |
| Zinc |
0.1
max |
| Density |
0.0968 lb/in3 |
| Hardness, Brinell |
60 |
| Tensile Strength |
33000 psi |
| Tensile Yield Strength |
28000 psi |
| Elongation at Break |
12 % |
| Modulus of Elasticity |
10200 ksi |
| Poisson's Ratio |
0.33 |
| Fatigue Strength |
17000 psi |
| Shear Modulus |
3760 ksi |
| Shear Strength |
20000 psi |
| Electrical Resistivity |
4.99e-006 ohm-cm |
| CTE, linear 68°F |
13.2 μin/in-°F |
| CTE, linear 250°C |
14.3 μin/in-°F |
| Specific Heat Capacity |
0.21 BTU/lb-°F |
| Thermal Conductivity |
960 BTU-in/hr-ft2-°F |
| Melting Point |
1125 - 1200 °F |
<<