360 Brass Data
| Density |
0.307 lb/in3 |
| Hardness, Rockwell B |
80 |
| Tensile Strength |
68200 psi |
| Tensile Strength, Yield |
52200 psi |
| Elongation at Break |
18 % |
| Modulus of Elasticity |
14100 ksi |
| Poisson's Ratio |
0.311 |
| Shear Modulus |
5370 ksi |
| Shear Strength |
37700 psi |
| Electrical Resistivity |
6.6e-006 ohm-cm |
| CTE, linear 250°C |
11.4 μin/in-°F |
| Specific Heat Capacity |
0.0908 BTU/lb-°F |
| Thermal Conductivity |
798 BTU-in/hr-ft2-°F |
| Melting Point |
1630 - 1650 °F |
| Annealing Temperature |
797 - 1110 °F |
| Hot-Working Temperature |
1290 - 1470 °F |
<<