260 Brass Data
| Density | 0.308 lb/in3 |
| Hardness, Rockwell B | 70 |
| Tensile Strength, Ultimate | 61600 psi |
| Tensile Strength, Yield | 52200 psi |
| Elongation at Break | 23 % |
| Modulus of Elasticity | 16000 ksi |
| Poisson's Ratio | 0.375 |
| Fatigue Strength | 18100 psi |
| Shear Modulus | 5800 ksi |
| Shear Strength | 39900 psi |
| CTE, linear 250°C | 11.1 μin/in-°F |
| Specific Heat Capacity | 0.0896 BTU/lb-°F |
| Thermal Conductivity | 833 BTU-in/hr-ft2-°F |
| Melting Point | 1680 - 1750 °F |
| Annealing Temperature | 797 - 1380 °F |
| Hot-Working Temperature | 1340 - 1560 °F |