Steel Threaded Rod Data
Mechanical Properties |
||||
|
||||
Hardness, Rockwell B | 60 | 60 | Converted from Brinell hardness. | |
Tensile Strength, Ultimate | 365 MPa | 52900 psi | ||
Tensile Strength, Yield | 305 MPa | 44200 psi | ||
Elongation at Break | 20 % | 20 % | In 50 mm | |
Modulus of Elasticity | 205 GPa | 29700 ksi | Typical for steel | |
Poisson's Ratio | 0.29 | 0.29 | Typical For Steel | |
Shear Modulus | 80 GPa | 11600 ksi | Typical for steel | |
Electrical Properties |
||||
|
||||
Electrical Resistivity | 1.43e-005 ohm-cm | 1.43e-005 ohm-cm | condition unknown | |
Thermal Properties |
||||
|
||||
CTE, linear 20°C | 12.2 μm/m-°C | 6.78 μin/in-°F | 0-100°C | |
CTE, linear 250°C | 13.5 μm/m-°C | 7.5 μin/in-°F | 0-300°C (68-570°F) | |
CTE, linear 500°C | 14.2 μm/m-°C | 7.89 μin/in-°F | 0-500°C (68-930°F) | |
Specific Heat Capacity | 0.448 J/g-°C | 0.107 BTU/lb-°F | condition unknown; 50-100°C (122-212°F) | |
Specific Heat Capacity at Elevated Temperature | 0.825 J/g-°C | 0.197 BTU/lb-°F | condition unknown; 650-700°C (1200-1290°F) | |
Thermal Conductivity | 49.8 W/m-K | 346 BTU-in/hr-ft2-°F |