420 Stainless Steel Technical Data
| Chemical
Composition |
| Carbon |
0.15
min |
| Chromium |
12
- 14 |
| Iron |
Balance |
| Manganese |
1
max |
| Phosphorus |
0.04
max |
| Silicon |
1
max |
| Sulphur |
0.03
max |
|
| Density |
0.282 lb/in³ |
| Hardness,
Rockwell B |
92 |
| Tensile
Strength |
95000 psi |
| Tensile
Strength, Yield |
50000 psi |
| Elongation
at Break |
20 % |
| Modulus
of Elasticity |
29000 ksi |
| Poisson's
Ratio |
0.24 |
| Charpy
Impact |
73.8 ft-lb |
| Shear
Modulus |
11700 ksi |
| Electrical
Resistivity |
5.5e-005 ohm-cm |
| CTE,
linear 20°C |
5.72 µin/in-°F |
| CTE,
linear 250°C |
6 µin/in-°F |
| CTE,
linear 500°C |
6.5 µin/in-°F |
| Specific
Heat Capacity |
0.11 BTU/lb-°F |
| Thermal
Conductivity |
173 BTU-in/hr-ft²-°F |
| Melting
Point |
2650
- 2750 °F |
| Maximum
Service Temperature, Air |
1150 °F |
| |
|